摘要
The incompact long afterglow pigment SrAl2O4: Eu, Dy was synthesized by ceramics technology.The agglomerated starting raw material had little effect on the synthesis of SrA12O4 matrix through solid-state reaction method,but the shrinkage and densification was retarded greatly by the agglomerated powder by the formation of large and extensive pore network.The sintering mechanism is surface diffusion ( without flux B2O3 ) and grain boundary diffusion (with B2O3 as flux)respectively, and the as-prepared long afterglow pigment glows in the dark for over 4000 min.