摘要
利用AOT/环己烷 /Cd(NO3 ) 2 微乳液通过TAA和H2 S为沉淀剂分别制备了超细CdS粒子 ,其尺寸达到纳米级 。
Preparation of ultrafine CdS particles was from microemulsion of AOT/cyclohexane/Cd(NO 3) 2 by precipitating agent of TAA and H 2S,The method was better than others because size reaching nm.