摘要 在600℃左右进行时效处理,可使针状铁素体管线钢强度水平大幅度提高而基本不降低韧性和延性.在600℃保温10 h,针状铁素体管线钢在保持塑、韧性的基础上,强度水平提升到接近X 100级别要求,且明显改善了其抗H2S开裂性能.有利作用主要归因于时效处理促进了针状铁素体中微合金碳氮化物的进一步沉淀析出,马氏体/奥氏体(M/A)岛转变成回火马氏体,以及组织更加均匀化.时效处理为发展高强度级别针状铁索体管线钢提供了新的思路. Hot-rolled acicular ferrite pipeline steel plate can be further strengthened by aging treatment. After an aging treatment at 600 degreesC for 10 h, the acicular ferrite pipeline steel plate is strengthened to the level of X 100 while its impact toughness does not obviously decrease. At the same time, its H2S cracking resistant ability is also improved obviously. All these can be attributed to the additional precipitation of micro-alloyed carbonitrides, the transformation of martensite/austenite (M/A) islands to tempering martensite and the improvement of the uniformity in acicular ferrite microstructure during aging treatment.
出处 《金属学报》 SCIE EI CAS CSCD 北大核心 2004年第9期948-954,共7页 Acta Metallurgica Sinica
基金 国家重点基础研究发展规划项目G1998061511
关键词 管线钢 针状铁素体 力学性能 抗H2S开裂性能 pipeline steel acicular ferrite mechanical property H2S resistance
  • 相关文献

参考文献10

  • 1[1]Kaneko T, Ikeda A. Trans Iron Steel Inst Jpn, 1988; 28:575
  • 2[2]Margot-Marette H, Bardou G, Charbonnier J C. Corros Sci, 1987; 27:1009
  • 3[4]Echaniz G, Morales C, Perez T. In: Corrosion/98, Houston, Texas: NACE, 1998:120
  • 4[5]Watkins M, Ayer R. In: Corrosion/95, Houston, Texas:NACE, 1995:50
  • 5[6]Ikeda A, Kowaka M. Chem Econ Eng Rev, 1978; 10:1
  • 6[7]Lopez H F, Bharadwaj R, Albarran J L, Martinez L. Metall Mater Trans, 1999; 30A: 2419
  • 7[8]Zhao M C, Tang B, Shan Y Y, Yang K. Metall Mater Trans, 2003; 34A: 1089
  • 8[10]NACE Standard TM0177-96, Laboratory Testing of Metals for Resistance to Specific Forms of Environmental Cracking in H2S Environments, 1996, NACE
  • 9[11]Smith Y E, Coldren A P, Cryderman R L. Toward Iraproved Ductility and Toughness. Tokyo: Climax Molybdenum Company Ltd., 1972:119
  • 10[13]Yoshie A, Fujioka M, Watanabe Y, Nishioka K, Morikawa H. ISIJ Int, 1992; 32:395

同被引文献118

引证文献12

二级引证文献97

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部