利用粉煤灰(或煤矸石)、铬渣、A渣等工业废渣为原料在980~1100CF煅烧该新型贝利特水泥;影响水泥及其熟料强度的主要因素、水泥的性能,以及水泥具有较高强度和较好抗蚀性能的机理。
The production of a new belite cement which is sintered at 980~ 1100C by ultilizing industrial slags, such as fly-ash (or coal gangue). chrome-slag,'A' slag, etc. as raw material is described. Studies on the main factors influen cingcement and clinker strength, the cement property, and the mechanism that it is of high strength and good anti-corrosion ferformances are emphatically presented.
出处
《水泥》
CAS
1993年第3期1-5,共5页
Cement
关键词
工业废渣
水泥
熟料
贝利特水泥
Industrial slag
Cement clinker
Belite cement