摘要
铵型锌锰电池通过改变电解液组分、正极配方及控制合理的电芯水分,使R6电池3.9Ω和5.0Ω连续放电时间分别达到107min和143min,达到了高功率电池的水平。
The preparation of high-powered ammonium chloride battery was reported. By changing the component of electrolyte and the component of the anode and controlling the rational moisture of anode. 107 minutes and 143 minutes on continuous discharge of R6 battery at 3. 9 and 5. 0 were obtained respectively. So this battery came up to the advanced high-power battery standards.
出处
《电池》
CAS
CSCD
1995年第4期179-180,共2页
Battery Bimonthly