摘要 The electroless deposition of Ni68-Fe10.5-P21.5 alloy has been investigated. The crystallization behavior of the deposit was comparatively studied by using differential scanning calorimetry and X-ray diffractometry. The deposit transforms into a square Ni3P phase at 380. 0 ℃, then changes into a cubic FeNi3 phase at 490. 0 ℃. The microhardness, the size of the formed grains and the magnetic performance of the deposit increase with the increase of the heat treatment temperature below 500 ℃, then they decrease after this temperature. The effect of heat treatment time at 500 ℃ on the surface micromorphology, the structure and the magnetic performance of the deposit were also studied. The resuits show that with the increase of heat treatment time, the extent of crystallization of the deposit increases and the size of the formed grains becomes uniform. The results also show that the magnetic performance of the deposit under heat treatment for 40 min is maximal and then decreases with the increase of heat treatment time. The property change of the deposit is related to the crystal structure and the size of the formed grains of the deposit. The electroless deposition of Ni68-Fe10.5-P21.5 alloy has been investigated. The crystallization behavior of the deposit was comparatively studied by using differential scanning calorimetry and X-ray diffractometry. The deposit transforms into a square Ni3P phase at 380. 0 ℃, then changes into a cubic FeNi3 phase at 490. 0 ℃. The microhardness, the size of the formed grains and the magnetic performance of the deposit increase with the increase of the heat treatment temperature below 500 ℃, then they decrease after this temperature. The effect of heat treatment time at 500 ℃ on the surface micromorphology, the structure and the magnetic performance of the deposit were also studied. The resuits show that with the increase of heat treatment time, the extent of crystallization of the deposit increases and the size of the formed grains becomes uniform. The results also show that the magnetic performance of the deposit under heat treatment for 40 min is maximal and then decreases with the increase of heat treatment time. The property change of the deposit is related to the crystal structure and the size of the formed grains of the deposit.
出处 《Chemical Research in Chinese Universities》 SCIE CAS CSCD 2005年第6期718-722,共5页 高等学校化学研究(英文版)
基金 SupportedbytheNaturalScienceFoundationofFujianProvince(No.E0210020).
关键词 Electroless plating Ni-Fe-P alloy Heat treatment Magnetic performance Electroless plating, Ni-Fe-P alloy, Heat treatment, Magnetic performance
  • 相关文献

参考文献14

  • 1Schmeckenbecher A. F., J. Electrochem. Soc., 1966, 113,778.
  • 2Schmeckenbecher A. F. , Plating, 1971, 58,905.
  • 3Freitag W. O. , Mathas J. S. , DiGuilio G. , J. Electrochem.Soc. , 1964, 111, 35.
  • 4Osaka T. , Electrochimica Acta, 1999, 44, 3885.
  • 5Matsuoka M. , Hayashi T. , Plat. and Surf. Fin. , 1982, 53.
  • 6KimD., MatsudaH., AokiK., Plat. &Surf. Fin. ,1996,78.
  • 7Sridharan K. , Sheppard K. , Trans. IMF. , 1994, 72(4), 163.
  • 8Sridharan K. , Sheppard K. , J. Appl. Electrochem. , 1997, 27,1198.
  • 9Wang L. L. , Zhao L. H. , Huang G. F. , et al. , Plat. & Surf.Fin. , 2001, 92.
  • 10WangL. L., ZhaoL. H., HuangG. F.,etal. ,Surf. &Coat.Tech. , 2000, 126, 272.

同被引文献57

引证文献4

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部