文章就江苏省杨溧高速公路某标段现浇高标号预应力砼连续箱梁裂缝产生的原因、施工应该注意的事项进行了较为详细的阐述,以供同类型桥梁施工参考。
The paper expounds on the causes of cracking in the cast-in-situ high grade prestressed concrete continuous box girders for a section of Yang-Li Express Highway in Jiangsu Province and precautions to be taken during the construction of the girders, which may be used as reference for construction of similar type of bridges.