改性砂浆砌体受剪性能的试验研究 被引量:1

Experimental Study of Shear Strength of Polymer Modification Grout Masonry
下载PDF
导出
摘要 新型墙体材料的广泛应用使得普通砂浆黏结性能差的局限性凸现.采用聚乙烯醇缩丁醛和甲基纤维素对普通砂浆做合理改性,进行了96个抗剪试件的正变试验,并对试验结果进行正变分析.结果表明:块体类别是最主要的影响因素,其次是聚合物掺量和砂浆强度;当聚乙烯醇缩丁醛和甲基纤维素的掺量分别为水泥质量的20%-30%和0.05%。0.1%时,可较大幅度提高砂浆的黏结强度. The deficiency of bond capacity of traditional cement mortar is exposed when the new walling materials arc used widely. In this paper, polyvinyl- butyral(PVB) and methyl cellulose(MC) are chosen as chemical additives to amend the property of normal mortar, orthogonal tests of 96 pieces of shear specimens are carried out, then orthogonal analysis of test results is performed. The results indicate that the sort of walling material is the most important factor in bond capacity of mortar, the mixed quantity of polymer and mortar strength follows, and there is a remarkable increase in mortar bond strength when the mixed quantity of PVB and MC is 20% - 30% and 0.05% -0. 1% respectively.
出处 《郑州大学学报(工学版)》 CAS 2006年第1期48-50,共3页 Journal of Zhengzhou University(Engineering Science)
关键词 砂浆 新型墙体材料 粘结强度 正交设计 聚合物 mortar the new walling material bond strength orthogonal design polymer
  • 相关文献

参考文献6

二级参考文献13

共引文献138

同被引文献7

  • 1高桂兰,赵子赢,沈成忠.浅谈砂浆强度与砌体强度[J].煤炭技术,2004,23(8):77-78. 被引量:3
  • 2殷向红.砖砌体砂浆的饱满度黏结力[J].同煤科技,2004(3):43-43. 被引量:2
  • 3刘梦溪,马金荣,于得水,李法浩.影响砌筑砂浆强度的因素探讨[J].能源技术与管理,2005,30(6):65-66. 被引量:2
  • 4苑振芳,刘斌.我国砌体结构的发展状况与展望[C]//施楚贤.2000年全国砌体结构学术会议论文集.北京:中国建筑工业出版社,2000.
  • 5施楚贤.影响砖砌体强度的几个因素[C]//钱义良.砌体结构研究论文集.长沙:湖南大学出版社,1989:32-34.
  • 6中华人民共和国建设部.JGJ/T98-2000砌筑砂浆配合比设计规程[S].北京:中国建筑工业出版社,2001.
  • 7中华人民共和国建设部.JGJ70-90建筑砂浆基本性能试验方法[S].北京:中国建筑工业出版社,1991.

引证文献1

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部