摘要
针对影响氧化铝陶瓷活化钼锰法金属化的工艺因素,在配方、原料处理、涂敷方式、烧结等方面进行改进,提高工艺水平,保证质量稳定性、一致性。
In order to overcome the influence of the technology factor in active molybdenum-manganese metallization, the formulation, raw material treatment, painting method and sintering process are improved in alumina ceramics metallization, which can raise the technique level, product quality and uniform.