摘要
在低温下通过改变第一次和第二次氧化条件尝试性地生长了系列模板,结合扫描电镜(SEM)研究了模板的孔间距和孔径与制备条件的关系。结果表明模板的形貌经两步氧化已达到最佳,孔间距受到第一步氧化的调制,改变第二步氧化的条件可以制备出不同孔径的模板。并在此基础上分析了模板的形成机理。
A series of alumina template are fabricated through altering oxidation condition of the first-step and the second-step. Scanning electron microscopy is used to observeand characterize the inter-pore distance and the pore diameter. The results show that a two-step anodic oxidation is enough to get good micrograph. The inter-pore distance is determined by the first-step oxidation. Templates with different pore diameters can be prepared by altering the second-step oxidation condition. The growing mechanism of.alumina template is also discussed.
出处
《核技术》
EI
CAS
CSCD
北大核心
2007年第3期171-173,共3页
Nuclear Techniques
基金
国家自然科学基金(10374087)项目支持
关键词
氧化铝模板
阳极氧化
制备方法
扫描电镜
Alumina template, Anodic oxidation, Preparing method, Scanning electron microscopy