针对某含钨、钼尾矿进行了试验研究,确定了浮选工艺条件,通过小型闭路试验获得白钨精矿含WO356.45%、回收率为70.23%;钼精矿含钼Mo48.50%、回收率58.20%的指标。
An experimental research on the tailings containing molybdenum and tungsten was carried out and the flotation process conditions were determined. The closed circuit test achieved the following indexes: WO3 grade in scheelite concentrate was 56.45 % and WO3 recovery reached 70.23 % ; Mo grade in molybdenum concentrate was 48.50% and Mo recovery reached 58.20%.