摘要
根据焊丝钢ER50-6用户对硫含量的要求,对精炼工序脱硫影响因素进行讨论,研究制定了生产该钢种的工艺路线、精炼工序的关键控制点。生产出的ER50-6钢硫含量达到了用户要求。
According to the requirement of users of ER50-6 welded wire steel on sulfur content,the desulfur factors during the refining procedure are discussed,and the technological flow and key control points of refining procedure made out,which to make the sulfur content of ER50-6 steel reaching the requirements of users.
出处
《天津冶金》
CAS
2007年第4期24-25,共2页
Tianjin Metallurgy
关键词
焊丝钢
冶炼
硫含量
控制
welded wire steel
sulfur content
smelting
control