摘要
研究了低钙水泥的制备,着重研究了低钙硅酸盐水泥和低铝贝利特硫铅酸盐水泥的配料和活化方法,得出掺加少量BaSO_4、SO_3和Na_2O都有活化贝利特水泥的作用,而以BaSO_4和SO_3的活化作用最好,可生产500~700号熟料。
The authors have made a study of low calcium cement production and emphatically have studied the raw mix design of low calcium Portland cement and low aluminium belite sulphoaluminate cement and activation meth ods.The activating action for belite cement can be obtained by adding a small amount of BaSOa_4,SO_3 and Na_2O.Among them,the activating action of BaSO_4 and SO_3 is the best and clinker of 500~700 grade can be produced.