摘要
B4C was added into the low-carbon MgO-C materials in order to improve the oxidation resistance. The results show adding 0. 3wt% B4C can get the best oxidation resistance and adding 0. 2 wt% B4C can get the highest hot modulus of rupture. Altogether, adding 0. 2wt% B,C into the low-carbon MgO-C materials can get better oxidation resistance and hot strength.
B4C was added into the low-carbon MgO-C materials in order to improve the oxidation resistance. The results show adding 0. 3wt% B4C can get the best oxidation resistance and adding 0. 2 wt% B4C can get the highest hot modulus of rupture. Altogether, adding 0. 2wt% B,C into the low-carbon MgO-C materials can get better oxidation resistance and hot strength.