摘要
在激光表面重溶预处理的TC4合金基材上预置涂敷CaHPO42H2O-CaCO3-Y2O3混合粉末,再经激光熔覆处理制备了生物陶瓷复合涂层。研究了该生物陶瓷涂层的织织和性能。结果表明,采用激光表面重熔预处理作过渡层制备的生物陶瓷涂层的界面结合良好,表层为HA和β-TCP组成的活性生物陶瓷复合涂层。
The bioceramic coating was made by Lasser remelt pretreating a layer of mixed powder CaHPO 4·2H 2O CaCO 3 Y 2O 3 on the TC 4 substrate.Effect of laser remelting preatment on microstuctures and properties was studied by SEM ESD XRD etc.The results show that laser remelting pretreatment is favorable to improvement of the mechanical properties and biocompatibility of bioceramic coating.
出处
《粉末冶金技术》
EI
CAS
CSCD
北大核心
1997年第3期195-198,共4页
Powder Metallurgy Technology
基金
国家自然科学基金
关键词
生物陶瓷
激光重熔
涂层
bioceramic,laser remelting,coating