期刊文献+

无缝钢管内折缺陷的研究 被引量:2

Research on Internal Folding Defect of Seamless Steel Pipe
下载PDF
导出
摘要 钢管内折缺陷一直是影响无缝厂400轧制作业区生产的主要原因。为了探索内折缺陷成因,从连铸坯、轧卡样、内折缺陷成品试样等进行现场试验并进行性能、低倍组织分析,总结产生钢管内折缺陷的原因。 Internal folding defect is a major factor which affects production of 400 rolling chance of seamless steel pipe. In order to find the reason of internal folding defect, the bloom, abandoned rolled seamless steel pipe and internal folding defect samples were collected. Experiments were carried and samples' performance and macrostructure were discussed. Based on it, the reasons of generating internal folding defects are summarized.
出处 《中国材料科技与设备》 2008年第1期95-96,104,共3页 Chinese Materials Science Technology & Equipment
关键词 无缝钢管 内折 缺陷 Seamless steel pipe Internal folding Defect