摘要
利用差示扫描量热(DSC)测出了低碳合金钢经高压处理后不同加热速率下组织中珠光体向奥氏体转变的温度和时间,并计算了其相变激活能。所得结果为研究低碳合金钢经高压处理后组织中珠光体向奥氏体转变提供一定的参考数据。
The phase transformation temperature and time from pearlite to austenite in low carbon alloy steel after high pressure treatment at different heating rates were measured by differential scanning calorimetry (DSC), and the activation energy was also calculated. As a result, it provides basis for studying phase transformation from pearlite to austenite in low carbon alloy steel after high pressure treatment.
出处
《热加工工艺》
CSCD
北大核心
2008年第14期45-46,49,共3页
Hot Working Technology
关键词
低碳合金钢
珠光体转变奥氏体
DSC
高压
low carbon alloy steel
transformation from pearlite to austenite
DSC
high pressure