摘要
通过对在库尔勒灰棕荒漠土中进行的铜、铅、铝短期自然埋藏试验的研究,分析总结了腐蚀原因和腐蚀规律。结果表明,灰棕荒漠土的质地不均易引发局部腐蚀,高含量的可溶性盐和微生物的活动对腐蚀有一定的促进作用。
Cu, Pb, and Al were naturally buried in the gray-brown desert soil of Kuerle, and the short-term soil corrosion mechanism and rule were summarized. The result showed that in gray-brown desert soil, the uneven texture of soil triggers local corrosion and high content of soluble salt and activities of microbes accelerate corrosion remarkably.
出处
《装备环境工程》
CAS
2008年第5期21-24,共4页
Equipment Environmental Engineering
基金
国家自然科学基金重大项目(50499333)
科技部国家科技基础条件平台项目(2005DKA10400)
科技部社会公益专项项目(2004DIBZJ058)
关键词
库尔勒荒漠土
铜
铅
铝
短期腐蚀行为
Kuerle desert soil
Cu
Pb
AI
short-term corrosion behavior