摘要
介绍了马钢二铁总厂通过优化配矿方案、提高炉内氧化气氛、改善透气性等措施,球团矿FeO含量由1.36%降低到0.72%的生产实践。
In this paper, the production practice of pellet mate-mine project, advancing shaft furnace oxidation ambience, improving permeability of Magang was summarized. The FeO content of pellet was reduced from 1.36% to 0.72%.
出处
《安徽冶金科技职业学院学报》
2009年第3期1-3,共3页
Journal of Anhui Vocational College of Metallurgy and Technology
关键词
球团矿
FEO含量
配矿
氧化气氛
透气性
pellet, FeO content, mate- mine, oxidation ambience, permeability