环保型含Bi低碳高硫易切削钢的开发 被引量:10

Development of Environment-friendly Containing Bi Low-Carbon High-Sulfur Free-Cutting Steel
下载PDF
导出
摘要 开发Bi易切削钢1215M(%:0.06C、0.04Si、1.25Mn、0.39S、0.17Bi)替代Pb易切削钢SUM24L。生产Bi易切削钢的流程为40t UHP EAF-40t LF(喂Bi线)-180 mm×180 mm连铸-连轧工艺。试验结果表明,Bi易切削钢1215MΦ9 mm盘条夹杂物分布均匀,Bi易切削钢1215M的切削性能优于SUM23HS含S易切削钢与SUM24L含Pb易切削钢相当。 Bi free-cutting steel 1215M (% : 0. 06C, 0. 04Si, 1.25Mn, 0. 39S, 0. 17Bi) has been developed to replace Pb free-cutting steel SUM24L. The flow sheet for production of Bi free-cutting steel is 40 t UHP EAF- 40 t LF ( feeding Bi wire)-180 mm × 180 mm CC-continuous rolling process. Test results show that the distribution of inclusions in Ф9 mm coil of Bi free-cutting steel 1215M is homogeneous, and the cutting performance of Bi free-cutting steel 1215M is better than that of S free-cutting steel SUM23HS and is equal to Pb free-cutting steel SUM24L.
出处 《特殊钢》 北大核心 2009年第6期23-25,共3页 Special Steel
关键词 易切削钢 低碳高硫 BI Free-Cutting Steel, Low-Carbon High Sulfur, Bi
  • 相关文献

参考文献1

二级参考文献3

  • 1王谦,谢兵,迟景灏.含硫易切钢连铸过程中的物化现象[J].连铸,1996,0(1):12-16. 被引量:9
  • 2张静纬.易切削钢的新技术和发展方向[J].天津冶金,2003,(3):59-59.
  • 3RamaBommaraju.易切削钢连铸坯纵裂及凹陷的成因及预防[A]..第一届欧洲连铸会议译文集[C].弗罗伦萨 意大利,1991.81-389.

共引文献6

同被引文献77

引证文献10

二级引证文献35

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部