摘要
介绍采用溶液聚合法以魔芋淀粉与丙烯酸接枝共聚制备高吸水性树脂的方法。通过单因素实验研究了反应温度、原料配比、反应条件等对吸水率的影响,确定了最佳反应条件,并测定产品的吸水率为780 g/g。
A super absorbent resin was prepared by graft copolymerization of konjac starch and acrylic acid.Single factor test indicates reaction temperature,amount of acrylic acid,amount of initiator,amount of water,etc.The optimum synthesis conditions were determined.The copolymer prepared can absorb deionized water 780g/g.
出处
《武汉工业学院学报》
CAS
2009年第4期48-51,共4页
Journal of Wuhan Polytechnic University
关键词
高吸水性树脂
魔芋淀粉
丙烯酸
接枝共聚
super absorbent resin
konjac starch
acrylic acid
copolymerization