摘要
The present paper reports the testing of 14 OPC-slag mortars and 2 controls OPC and slag mortars. The main aim is to determine the optimum level of replacement slag for achievement to the highest early strength with reasonable flow. Variable was the level of GGBFS in the binder. In this experimental work, two types of sands were used that are: silica and mining sands. It is determined that the optimum level of replacement slag is 40% and use of silica sand in OPC is preferable to mining sand and reversely, use of mining sand is preferred in GG100 to silica sand. All mortars had W/B and S/B 0.33 and 2.25, respectively.