摘要
在批量检测过程中遇到测区强度值小于10MPa的情况时,如果采用钻芯修正的方法将无法继续计算下去。采用逐级调整碳化的方法来解决含有测区强度值小于10MPa的批量的修正,可使该批量得到具体的数据,以方便设计的验算。
Can meet in the batch examination process measured the area intensity value is smaller than the 10MPa situation, if by now will use drills the method which the core revised to be unable to continue to calculate. Uses the method which the progressive adjustment carbonizes to solve includes measured the area intensity value is smaller than the 10MPa batch revision, may obtain this batch the concrete data, has facilitated the design the checking calculation.
出处
《工程建设与设计》
2010年第4期31-34,共4页
Construction & Design for Engineering
关键词
批量检测
测区强度小于10MPa
调整碳化
钻芯修正
batch examination
measured the area intensity is smallerthanl OMPa
adjustmentcarbonization
drills the core to revise