期刊文献+

转炉增碳法连铸生产45钢高线工艺的冶炼参数研究 被引量:8

STEELMAKING PARAMETERS OF 45 STEEL WIRE ROD USED FOR HIGHSPEED ROLLING PRODUCED BY RECARBURIZING IN LADLE AND CC
下载PDF
导出
摘要 马鞍山钢铁股份有限公司于1997年采用转炉增碳法连铸生产45钢高线。冶炼工艺采用深吹加炉后增碳法,通过炉内操作制度的优化和炉后脱氧制度的改变及合理的工艺参数控制,生产了满足连铸要求的钢水,最终产品成分均匀、通条性能稳定。本文就生产和试验数据,探讨了该工艺冶炼部分的工艺控制参数。 The experimental investigation and commercial production of the 45 steel wire rod used for highspeed rolling by recarburizing after tapping in the ladle and CC have been proceeded since 1997 The key parameters of steelmaking and casting processes are investigated The molten steel meeting the requirement for CC is made by deep blowing in the converter with downstream recarburization and deoxidation in the ladle The finished product has features of homogeneous composition,good mechanical behavior and homogeneous all coil properties Based on the experimental and operational result,the optimal technological parameters are discussed
作者 马玉平
出处 《钢铁》 CAS CSCD 北大核心 1999年第1期12-15,26,共5页 Iron and Steel
关键词 转炉 增碳法 炼钢 碳钢 冶炼参数 氧气顶吹转炉 steel 45, BOF steelmaking,recarburization
  • 相关文献

参考文献3

共引文献13

同被引文献49

引证文献8

二级引证文献13

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部