摘要
分别采用4种离析液(a.HNO3-KClO3、b.NaClO、c.H2O2-HAc、d.NaOH)对一年生慈竹进行离析,研究不同化学离析方法、离析时间及超声等条件下对纤维接触角和纤维中空的影响。结果表明:不同离析方法的离析时间(t)差别较大,ta<tb<td<tc;离析出的纤维接触角(C)不同,Ca<Cd<Cb<Cc;纤维中空(H)有较大差异,Hc<Hd;离析过程中,超声波能够加快离析速度,缩短离析时间,降低纤维接触角。
Annual Neosinocalamus affinis was treated in four kinds of maceration (a), NaCIO (b), H2O2-HAc (c) and NaOH (d), respectively. solutions, i.e. HNO3-KCIO3 Effects of different chemical maceration methods, maceration time and ultrasonic test on contact angle of single fiber and hollow fiber were studied. The results showed that the maceration time of four methods was largely different (ta 〈 tb 〈 td 〈 tc) , contact angles of single fiber were dissimilar ( Ca 〈 Cd 〈 Cb 〈 C ) and hollow fibers were diverse (Hc 〈 Hd). In the maceration process, ultrasonic wave can accelerate the maceration rate, shorten the maceration time and reduce the contact angle of single fiber.
出处
《北京林业大学学报》
CAS
CSCD
北大核心
2011年第1期115-118,共4页
Journal of Beijing Forestry University
基金
"十一五"国家科技支撑计划项目(2006BAD19B07)
"948"国家林业局引进项目(2006-4-104)
林业引智项目(20100327024)
国家自然科学基金重点项目(30730076)
关键词
离析方法
接触角
离析时间
纤维中空
maceration method
contact angle
maceration time
hollow fiber