跑气保用轮胎胎侧支撑胶配方的优化设计 被引量:1

Optimized Formula Design of Side-reinforcing Compound for Run-flat Tire
下载PDF
导出
摘要 对跑气保用轮胎胎侧支撑胶配方进行优化设计。试验结果表明:在胎侧支撑胶配方中采用补强树脂部分替代炭黑,并加入适量促进剂HMT,得到优化配方为:NR/BR70/30,炭黑N37550,氧化锌5,硬脂酸2,补强树脂SP67016,防老剂4020/RD3,硫黄3,促进剂HMT0.6,其他5.7。采用优化配方的硫化胶弹性和耐屈挠性能较好,生热较低,工艺性能良好,成品轮胎零气压下的耐久性能超过了设计要求。 The formula design of side-reinforcing compound for run-flat tire was optimized,in which carbon black was partly replaced by reinforcing resin and addition level of accelerator HMT was adjusted.The optimized formula was as follows:NR/BR 70/30,carbon black N375 50,zinc oxide 5,stearic acid 2,reinforcing resin SP6701 6,antioxidant 4020/RD 3,sulfur 3,accelerator HMT 0.6,other components 5.7.The elasticity and flexing resistance of the optimized vulcanizate were improved,the heat build-up was lower,the processibility was good,and the endurance of finished tire under zero pressure exceeded the design specification.
出处 《轮胎工业》 CAS 2011年第2期102-104,共3页 Tire Industry
关键词 跑气保用轮胎 胎侧支撑胶 补强树脂 run-flat tire side-reinforcing compound reinforcing resin
  • 相关文献

同被引文献5

引证文献1

二级引证文献12

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部