摘要
采用转炉→LF→RH→连铸→热轧→酸洗→冷轧→退火→精整的工艺路线,通过严格控制C含量,制定合理的工艺参数,生产的Ti-IF冲压用St14钢带产品具有均匀的铁素体组织,良好的综合力学性能和深冲性能,平均r值为2.2,能满足复杂冲压件的使用要求。
Adopting the process route of converter-LF-RF-hot rolling-annealing-finishing and through controlling the content of carbon strictly and establishing reasonable process parameters,Ti-IF steel for stamping St14 strip was produced.The metallographic of the products with good comprehensive mechanical properties and deep drawability is uniform ferrite.The average plastic strain ratio is 2.2 and can be used to produce complicated stamping parts.
出处
《山东冶金》
CAS
2011年第2期21-22,共2页
Shandong Metallurgy
关键词
TI-IF钢
St14
冷轧钢带
成分控制
生产工艺
塑性应变比
Ti-IF steel
St14
cold rolled steel strip
compositional control
production process
plastic strain ratio