摘要 用HIOKI3551 电池内阻测试仪对大容量(> 100Ah)阀控式密封铅酸蓄电池的内阻及其影响因素进行了研究。研究表明,在10 h 率放电过程中,剩余容量高于50% 时,电池内阻变化不大(仅增大5% );并且内阻和放电时间可拟合为指数函数Rt= R0 + C1 ×exp(t/C2)。极板只有与汇流排完全断开,内阻才会明显增大。蓄电池温度在- 40~0℃和0~50℃时,随温度上升,蓄电池电导线性增加。在0~50 kPa时,电池内部压力每增大10kPa,内阻增大3 μΩ。另外,接触电阻对测试值有一定影响。 The internal resistance of VRLA batteries with high capacity (more than 100 Ah) and the effective factors were studies with HIOKI 3551 battery tester. The results show that the internal resistance rises a little (only 5%) when the residual capacity is more than 50% and the correlation between the internal resistance and the discharge time can be indicated as an exponential function of R t=R 0+C 1×exp(t/C 2) during discharge at C 10 rate. The internal resistance will rise sharply just when plates are completely broken at the lugs. There is a linear correlation between the conductance and the battery temperature when it varies from -40℃ to 50℃. The internal resistance will rise 3 μΩ with the gas pressure rising 10 kPa. In addition, the contact resistance also influences the test value.
出处 《电源技术》 CAS CSCD 北大核心 1999年第6期302-303,331,共3页 Chinese Journal of Power Sources
关键词 铅酸蓄电池 内阻 电导 阀控式蓄电池 VRLA internal resistance/conductance residual capacity State of Health temperature pressure
  • 相关文献

参考文献5

二级参考文献2

共引文献31

同被引文献126

引证文献24

二级引证文献114

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部