摘要 在电气线路火灾原因的调查中,为更好地区分铜导线一次短路与二次短路的熔痕特征,用扫描电子显微镜(SEM)和X-射线能谱仪(EDS)对2种熔痕的形貌和相应的元素成分进行了试验研究。结果表明:铜导线一次短路与二次短路熔痕的表观形貌特征和元素成分具有明显的不同,二者的区别主要表现在熔痕表面所含的气孔、元素种类及导线本体与熔痕之间的过渡区方面,一次短路熔痕表面气孔多,元素种类少,导线与熔痕之间有明显界限,二次短路熔痕则相反。该研究结果可以区分短路熔痕形成的环境气氛,以此判断导线短路熔痕类型,为电气线路火灾原因的调查提供科学依据。 For distinguishing the primary and secondary short-circuit melted mark of copper wires better during the electrical fire investigation,SEM and X-ray EDS were used to observe their morphology and corresponding component elements.The results show that the characteristics of their morphology and component elements are clearly different.And their major differences are the pores and element species on the melted mark surface,as well as the transition region between the original wire and the melted mark.These conclusions can be used to identify the style of the melted mark by distinguishing their forming atmosphere,providing a scientific basis and a new technical method for electrical fire investigation.
作者 文玉秀 王敏
出处 《中国安全科学学报》 CAS CSCD 北大核心 2011年第6期84-87,共4页 China Safety Science Journal
关键词 铜导线 扫描电子显微镜/射线能谱仪(SEM/EDS) 短路熔痕 成分分析 copper wire scanning electron microscope(SEM)/energy dispersive spectrometer(EDS) short circuit melted mark component analysis
  • 相关文献

参考文献8

二级参考文献3

  • 1公安部消防局.火灾事故调查(培训教材)[M].长春:吉林科学技术出版社,1999..
  • 2王希庆 等.电气火灾现场勘查和鉴定技术指南[M].沈阳:辽宁大学出版社,1996..
  • 3赵长征.电气火灾原因认定和痕迹鉴定[J].消防技术与产品信息,2003,16(12):3-5. 被引量:32

共引文献136

同被引文献83

引证文献7

二级引证文献26

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部