利用自行设计制造的半固态连铸机对Fe-Cr-C系及Fe-Mn-C系合金进行了半固态连铸试验。着重研究了工艺参数对拉漏及拉断现象的影响,探讨了拉漏拉断的条件及机理,提出了防止拉漏拉断的技术途径。
A series of continuous casting tests for Fe-Cr-C white cast iron and Fe-Mn-C high manganese steel were carried out with a self-made semisolid metal continuous casting machine. Based on the result, influence of process parameters on the breakout or breakage was studied. The condition and mechanism of breakout or breakage was discussed. The technical methods to prevent this defects were offered.
出处
《特种铸造及有色合金》
EI
CAS
CSCD
北大核心
2000年第1期16-19,共4页
Special Casting & Nonferrous Alloys
基金
河北省自然科学基金!(599281)
关键词
半固态连铸
拉漏
拉断
半固态连铸机
Semisolid Metal Continuous Casting, Breakout,Breakage,Mechanism