期刊文献+

X80管线钢生产过程纯净度控制

Production Process Control of Cleanliness in X80 Pipeline Steel
下载PDF
导出
摘要 介绍了采用铁水脱硫预处理、复吹转炉、LF精炼、RH精炼、板坯连铸工艺开发X80管线钢的过程。采用该工艺生产的X80管线钢钢水成品[C]≤0.05%[,P]≤0.012%[,S]≤0.0022%[,N]≤0.005%,T[O]≤30×10-6,[H]≤2.5×10-6,钢中的A、B类夹杂物控制在1.5级以下,C、D类夹杂物能控制在0.5级以下,管线钢洁净度完全满足用户要求。 This paper introduced the development course of X80 pipeline steel steelworks with hot metal pretreatment and combined blowing converter and LF refining and RH refining and the slab continuous casting. [C] are below 0.050%, [P] are below 0.0120% ,IS] are below 0.0020% ,[N] are below 0.0050% ,T [O] are below 30 × 10^-6 ,[H] are below 2.5 × 10^-6, respectively in XS0 pipeline steel produced by this craft, besides, A type and B type kinds of inclusions are con-trolled below 1.5 grade. C type and D type kinds of inclusions are controlled below 0.5 grade. Pipeline steel cleanliness absolutely satisfy consumer request, each mechanical properties absolutely satisfy domestic and overseas standard.
出处 《新疆钢铁》 2012年第1期11-14,共4页 Xinjiang Iron and Steel
关键词 X80管线钢 纯净度 气体 夹杂物 X80 pipeline steel cleanliness gas inclusion
  • 相关文献

参考文献2

二级参考文献3

共引文献8

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部