红土镍矿微波水热法浸提镍钴 被引量:11

Extraction of nickel and cobalt from laterite using a microwave assisted hydrothermal leaching method
原文传递
导出
摘要 采用微波水热盐酸浸出方法对腐泥土型红土镍矿提取镍钴进行了研究,详细探讨了焙烧预处理、微波水热浸出温度和浸出时间对镍钴浸出率的影响.对于300℃焙烧预处理后的红土镍矿,微波水热温度为50℃,浸出时间为1 h时,镍的浸出率高达93.65%,钴的浸出率为87.86%.红土镍矿的微波水热浸出体系与普通水热浸出体系相比,镍和钴的浸出效果更好.研究表明,扩散过程是镍、钴浸出过程的主要限制环节. A microwave assisted hydrothermal leaching method was used to extract nickel and cobalt from saprolite laterite. The effects of roasting pretreatment, leaching temperature and time on the extraction ratios of nickel and cobalt were investigated in detail. The extraction ratio of 93.65% for nickel and 87.86% for cobalt can be obtained respectively when the leaching temperature and time are 50 ℃ and 1h for saprolite laterite only pre-roasted at 300 ℃. Comparing the microwave assisted hydrothermal leaching method with a hydrothermal leaching method, nickel and cobah can be extracted more efficiently from the laterite. The experimental data indicate that the leaching process of nickel and cobalt is a diffusion-controlled process.
出处 《北京科技大学学报》 EI CAS CSCD 北大核心 2012年第6期632-638,共7页 Journal of University of Science and Technology Beijing
基金 国家自然科学基金资助项目(50872011) 国家重点基础研究发展计划资助项目(2007CB613608) 教育部新世纪优秀人才支持计划资助项目(NCET--08--0732)
关键词 红土镍矿 微波加热 水热法 提取 焙烧 laterite microwave heating hydrothermal methods extraction nickel cobalt roasting
  • 相关文献

参考文献19

二级参考文献81

共引文献213

同被引文献175

引证文献11

二级引证文献93

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部