期刊文献+

某选铁尾矿回收铁的选矿工艺研究 被引量:9

Research on Recovering Iron from Iron-Separation Tailings
下载PDF
导出
摘要 某选铁尾矿含铁28.04%,该尾矿主要是选铁洗矿过程中的溢流部分,其粒度非常细。针对该尾矿特点,进行回收铁的试验研究。通过多方案的对比,最终采用矿浆分散-磁选-浮选的联合试验流程,其闭路试验可得到含铁58.77%的铁精矿,铁回收率68.58%,使该尾矿资源得以综合利用,提高了企业的经济和社会效益。 An iron-separation tailings containing Fe 28.04% is the overflow in the washing processing and its size is really fine.This paper studied on the iron recovery of the tailings.The combination experiment flow of ore pulp dispersion,magnetic separation and floatation was adopted after Comparing with several schemes.The closed-circuit testing is as following: the iron concentrate grade is 58.77%and the iron recovery rate is 68.58%.So it makes the tailings be used comprehensively and improves the enterprise with economic and social benefits.
作者 张红英
出处 《铜业工程》 CAS 2012年第4期15-17,21,共4页 Copper Engineering
关键词 溢流 尾矿 矿浆分散-磁选 磁浮联合 综合利用 overflow tailings pulp dispersion-magnetic separation combination of magnetic separation and floatation comprehensive utilization
  • 相关文献

参考文献6

二级参考文献20

共引文献51

同被引文献152

引证文献9

二级引证文献77

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部