摘要
在对西藏某复杂难选铜锌硫化矿进行矿石性质分析的基础上,按优先浮铜再选锌的原则流程首先分别进行了铜、锌矿物粗选及精选工艺技术条件研究,然后进行闭路流程试验,获得了铜品位为20.10%、回收率为70.26%、含银90.20 g/t的铜精矿,锌品位为42.33%、回收率为75.35%、含银14.80 g/t的锌精矿,铜锌分离效果较好,但富集在铜精矿、锌精矿中的银回收率有待提高。
Based on the study of the property of a complex copper-zinc sulfide ore from tibet, the process flowsheet of preferential flotation Cu and the railings of flotation Cu treated by flotation Zn was adopted and the technical conditions of Cu-Zn mineral roughing and cleaning were researched. A copper concentrate contenting copper 20. 10% with recovery 70. 26% and contenting silver 90. 20 g/t, a zinc concentrate contenting zinc 42. 33% with recovery 75.35% and contenting silver 14. 80 g/t can be obtained by the finally definitive closed circuit test. Although the copper-zinc separation was successful realized, the recovery of silver in copper, zinc concentrate needs to be further improved.
出处
《金属矿山》
CAS
北大核心
2012年第9期57-60,79,共5页
Metal Mine
关键词
复杂铜锌硫化矿
优先浮选
铜锌分离
组合抑制剂
Copperzinc complex sulfide minerals, Preferential flotation, Copper-zinc separation, Combined depressor