摘要
针对邢台魏鲁地区蓝晶石尾矿中长石含量较高,铁品位为0.98%,采用强磁-浮选提纯方法进行了除铁试验研究,得到长石精矿的Fe2O3含量降为0.09%。
The low-grade feldspar from kyanite tailings were studied through the magnetic - Anti-flotation purification method. The ore grade of iron was degraded from 0.98% to 0.09%.
出处
《非金属矿》
CAS
CSCD
北大核心
2013年第1期36-37,共2页
Non-Metallic Mines
关键词
长石
强磁选
浮选
蓝晶石尾矿
feldspar magnetic separation flotation kyanite tailings