通过改善结合剂的耐火度、流动性、强度,试制出用于低温烧成(1000℃以下)的低熔结合剂。该结合剂的强度和制作成的试块的硬度都比较高。
By improving the refractoriness,refractoriness,and strength of bonds, we have trial-produced Low-melting bond sample block in Low-temperature sintering. The strength of bond and the hardness of sample block produced are all higher.
出处
《金刚石与磨料磨具工程》
CAS
2000年第4期27-28,共2页
Diamond & Abrasives Engineering
关键词
SiC磨具
低温烧成
低熔结合剂
强度
硬度
SiC abrasive products Low-temperature sintering Low-melting bond the strength and hardness of bond