对我国大兴安岭地区落叶松25~30mm厚锯材的快速干燥工艺基准进行了试验与探讨。通过试验与分析得知,试验所制定的干燥工艺基准能够满足该树种及规格锯材的木材干燥生产要求,其经济效益可观,木材干燥生产企业可以参考采用。
Tests and discussion about the quick drying process datum for 25-30mm thick larch timber in Daxing' anling area in Northeast China are conducted. Through tests and analysis, it is learned that the drying process datum determined during testing can meet the drying production requirements of this species and timber of this size, with considerable economic benefits, and such datum can be used by wood drying production enterprises for reference.