摘要
对新疆某高硅低品位难选赤铁矿石采用阶段磨矿、阶段高梯度强磁选—反浮选原则流程进行了开发利用工艺技术条件研究。结果表明,用磨矿—强磁粗选—粗精矿再磨—强磁精选—强磁精矿1粗1精反浮选、精选尾矿返回流程处理,可获得铁品位为61.10%、铁回收率为65.63%的铁精矿。
Ore dressing processes consisting of stage grinding-stage high gradient high intensity magnetic separation-re- verse flotation were applied for development and utilization of a high-silica low-grade hematte ore in Xinjiang. The results showed that ironc concentrate with Fe grade of 61.10% and Fe recovery of 65.63% was achieved throght the process flowshe- et of grinding-high intensity magnetic separation-regrinding of coarse concentrate-clean concentration by high intensity magan- tic separation-one roughing and one cleaning reverse floatation of the high intensity concentrate-middles back to the flowsheet.
出处
《金属矿山》
CAS
北大核心
2013年第9期72-75,共4页
Metal Mine
关键词
赤铁矿
强磁选
反浮选
Hematite, High intensity magnetic separation, Reverse flotation