摘要 采用氧化焙烧脱硫、除碳-碳酸钠溶液浸出钼-浸钼渣氰化提金新工艺处理某金钼混合精矿。结果表明,在下述最佳试验条件下:粗精矿于600℃氧化焙烧1.5h、钼焙砂加入矿重40%的碳酸钠后按液固比3~4在80~90℃浸出1.0~1.5h,钼浸出率为91%,浸钼渣金的氰化浸出率大于95%。 Low grade gold-molybdenum mixed concentrate was treated by new processes of desulfurization and decarbonization by oxidizing roasting, molybdenum leaching with sodium carbonate, and gold cyaniding from molybdenum leaching residue. The results show that molybdenum leaching rate is 91% when rough concentrate is oxidization roasted at 600 ℃ for 1.5 h, molybdenum calcining is leached at 80-90 ℃ for 1.0-1.5 h by sodium carbonate of 40% of weight of calcining with ratio of liquid to solid of 3-4. Gold cyaniding leaching rate from molybdenum leaching residue is 95 % above.
出处 《有色金属(冶炼部分)》 CAS 北大核心 2014年第7期42-44,63,共4页 Nonferrous Metals(Extractive Metallurgy)
基金 国土资源地质调查项目(1212011120305)
关键词 金钼混合精矿 氧化焙烧 碳酸钠 浸出 分离 gold-molybdenum mixed concentrates oxidizing roasting sodium carbonate leaching separation
  • 相关文献

参考文献8

二级参考文献40

共引文献38

同被引文献6

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部