对武钢乌龙泉矿石灰石的晶粒度和矿相组织进行了测试;同时在实验室竖式炉内用石灰石煅烧活性石灰。选取的参数为:煅烧温度和保温时间(煅烧时间)。研究了其对煅烧出的石灰活性度的影响。
The grain fineness and the ore phase of the limestone in Wulongquan mine was measured and the study on calcining active lime with experimental upright furnace was performed. The calcine temperature and lasting time were selected as technological parameter during the calcining process.The influence of these technological parameter on activity of the lime was researched.