Effect of the Binders' Burning out on Strength and Microstructure of Ceramic Green Bodies in the Course of Gelcasting
下载PDF
导出
摘要 研究了凝胶注成型过程中 ,排胶对坯体强度及其显微结构的影响 .研究发现 ,随着排胶温度的升高 ,排胶过程具有阶段性 :当温度低于 2 0 0℃时 ,坯体强度稍有下降 ;当温度升至 35 0~ 5 0 0℃时 ,由于坯体内部高分子网络逐渐软化、分解 ,强度显著下降 ;当温度高于 5 0 0℃时 ,由于坯体内部局部烧结 ,强度则逐渐回升 . The variation of strength and microstructure of green bodies were studied in the course of binders' burning out. The results show that the burnout course could be divided into three stages. When temperature is below 200 degree C, the mechanical properties of green bodies decrease with temperature increasing. When temperature increases to 350~500 degree C, the strength decreases sharply because the organic net formed in shaping course becomes softening and decompositing. And when temperature increases to 900 degree C, the strength increases gradually because of the partial sintering occured in the body.
出处 《西安交通大学学报》 EI CAS CSCD 北大核心 2001年第11期1198-1200,共3页 Journal of Xi'an Jiaotong University
基金 西安交通大学科学研究基金资助项目
关键词 陶瓷 机械性能 凝胶注成型 生坯强度 显微结构 排胶温度 ceramics gelcasting binders' burning out mechanical property
  • 相关文献

参考文献3

  • 1[1]Janney M A. Method for molding ceramic powder [P]. US Pate nt, 4894194.1990-01-06.
  • 2[2]Janney M A. Omatete O O. Method for molding ceramic powders using a wate r-based gelcasting [P]. US Patent, 528362. 1991-07-02.
  • 3[3]Omatete O O. Gel-casting, a new ceramic forming process [J]. Am Cera m Soc Bull, 1991, 70(10): 1 641~1 649.

同被引文献53

  • 1刘晓光,仝建峰,李宝伟,陈大明.水基凝胶注模坯体的排胶工艺研究[J].航空材料学报,2005,25(1):48-52. 被引量:5
  • 2郭文利,徐廷献,燕青芝,葛昌纯.N-羟甲基丙烯酰胺聚合体系注凝成型纳米氮化硅陶瓷[J].硅酸盐学报,2006,34(2):147-151. 被引量:15
  • 3胡艳,杜红炎.稀土掺杂对BaTiO_3陶瓷结构和性能的影响[J].四川稀土,2007(1):20-23. 被引量:1
  • 4NGUYEN Q MINH.Ceramic fuel cells[J].J Am Ceram Soc,1993,76(3):563-588.
  • 5SHOJAI F,MANTYLA T A.Effect of sintering temperature and holding time on the properties of 3Y-ZrO2 micro-filtration[J].J Mater Sci,2001,36:3437-3446.
  • 6RHODES W H.Controlled transient solid second phase sintering of yttria[J].J Am Ceram Soc,1987,64(1):13-19.
  • 7DAVID L BOURELL,PARIMAL.Sol-gel synthesis of na-nophase yttria-stabilized tetragonal zirconia and densification behavior below 1600K[J].J Am Ceram Soc,1993,76(5):705-711.
  • 8JANE W ADAMS.Flexural strength,and fracture of yttria-stabilized zirconia versus temperature[J].J Am Ceram Soc,1997,80 (4):903-908.
  • 9Si W J,Graule T J,Baader F H,et al.Direct coagulation lasting of sil[J].Am Ceram Soc Bull,1991,74(3):612~16.
  • 10Omatete O O,Janny M A,Strehlow R A.Gelcasting-a new ceramic forming process[J].Am Ceram Soc Bull,1991,70(10):1641~1649.

引证文献6

二级引证文献5

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部