摘要
通过 1 0 0℃干燥试验法的试验 ,获得了狄氏黄胆木木材的基本干燥特性数据。狄氏黄胆木木材的干燥特性是 :初期开裂与截面变形的干燥等级为 3级 ,内部开裂的干燥等级为 2级。根据这些特性因子编制了狄氏黄胆木板材的干燥基准。表 6参
Drying characters data contributive to drying technology research of Nauclea diderrichii was obtained through a series of tests with 100 ℃ drying test method.The results whowed that drying characteristics of Nauclea diderrichii are as following:Classifications of initial checks or cross section deformation are 3 and classification of inner checks is 2.The drying schedule of Nauclea diderrichii was made by these parameters of drying characteristics.
出处
《浙江林学院学报》
CAS
CSCD
北大核心
2001年第4期384-388,共5页
Journal of Zhejiang Forestry College
基金
浙江省教育厅资助项目 ( 2 0 0 0 0 5 90 )