大规格圆坯表面裂纹的控制 被引量:2

Control Surface Cracks for Large Round Billet
下载PDF
导出
摘要 包钢在生产大规格合金品种钢圆管坯时出现表面裂纹。文章从表面裂纹产生的特征开始分析,找出表面裂纹出现的原因,通过系统分析总结出消除圆坯表面裂纹的工艺措施。建议优化钢种成分提高热延展性,以合适的拉速匹配二冷区冷却制度,提高钢坯过矫直段温度,解决了圆坯表面裂纹的问题。 The round billet of large alloy variety steel manufactured by Baotou Steel is with the surface cracks. In the paper,the causes of them are found out through analyzing their features. Moreover,such technological measures as optimizing the steel components to improve the hot ductility and increasing the temperature of straightening section when billet is through it with the appropriate casting speed to match the cooling system of secondary cooling zone are summarized through systematic analysis as well as the problem is solved with them.
出处 《包钢科技》 2015年第5期22-24,共3页 Science & Technology of Baotou Steel
关键词 大规格圆管坯 表面裂纹 延展性 large round billet surface crack ductility
  • 相关文献

参考文献3

二级参考文献25

  • 1肖洪达.连铸坯裂纹产生的机理及预防[J].辽宁冶金,1994(2):24-28. 被引量:3
  • 2杨菊娣,殷碧群,解宝荣.Nb微合金化钢连铸坯表面裂纹[J].钢铁研究,1990,18(3):46-51. 被引量:6
  • 3蔡开科.连续铸钢[M].冶金工业出版社,1991,9..
  • 4蔡开科 党紫九.连铸钢高温力学性能[J].北京科技大学学报,1993,(2).
  • 5PAN Zhiguo,YI Guilan. Symposium of the 12th National Steelmaking Conference [ C ]. Beijing :2000,372 - 375.
  • 6蔡开科.连续铸钢原理与工艺[M].北京:冶金工业出版社,2002.311-312.
  • 7蔡开科.连续铸钢500问[M].北京:冶金工业出版社,1994.7.
  • 8宋维锡.金属学[M].北京:冶金工业出版社,1980..
  • 9Deisinger, K. H. Tacke, Unbending of continuously cast slabs with liquid core [ J ]. Ironmaking and steelmaking, 1997, Vol24(4) : 321 - 328.
  • 10邵璐.[D].北京:北京科技大学,1990.

共引文献28

同被引文献12

引证文献2

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部