摘要 利用哈克转矩流变仪研究再生温度对2种粒径范围的胎面胶粉和全胎胶粉再生橡胶再生效果的影响。结果表明:再生温度为185~190℃时,粒径为0.55~0.76和0.38~0.55 mm的胎面胶粉再生橡胶再生效果较好;再生温度为195~200℃时,粒径为0.55~0.76 mm的全胎胶粉再生橡胶再生效果较好;再生温度为190~195℃时,粒径为0.38~0.55 mm的全胎胶粉再生橡胶再生效果较好。 The influence of temperature on the regeneration effect of reclaimed rubber regenerated from two particle size ranges of tread rubber powder and ground whole tire rubber powder was investigated through Haake torque rheometer. The results showed that good regeneration results of tread rubber powder with the particle size of 0. 55~0. 76 and 0. 38~0. 55 mm was achieved at the temperature range of 185~190 ℃,while the preferable regeneration temperature ranges for the whole tire powder with particle size of 0. 55~0. 76 and 0. 38~0. 55 mm were 195~200 ℃ and 190~195 ℃,respectively.
出处 《橡胶工业》 CAS 2016年第10期619-622,共4页 China Rubber Industry
关键词 胎面胶粉 全胎胶粉 再生温度 再生橡胶 再生效果 tread rubber powder tire rubber powder regeneration temperature reclaimed rubber regeneration effect
  • 相关文献

参考文献1

二级参考文献6

共引文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部