摘要
研究微波协同纳米氧化锌抗菌试验的最佳工艺。在最佳工艺条件下,探讨了微波协同纳米氧化锌的最佳抗菌率,同时进行了纳米氧化锌的回收试验,并测定多次回收的纳米材料抗菌效果的变化规律。微波协同纳米氧化锌抗菌的最佳工艺为:纳米氧化锌与羽绒质量比为0.5,微波时间为3 min,微波功率为200 W,微波时温度50℃,最佳抗菌率为89.13%。微波协同纳米氧化锌对羽绒有较好的抗菌效果,至少可进行2次回收循环使用。
The optimum antibacterial process of down with nano-zinc oxide cobined with microwave is discussed, and the optimal antibacterial rate is analyzed. Meanwhile, the recycling of nano-zinc oxide is carried out, and the law of the sterilization rate of the recycled materials is exploited. The results show that the optimum antibacterial conditions are: the ratio of nano-zinc oxide to feather mass 0. 5, radiation time 3 min, radiation power 200 W and radiation temperature 50℃, and the best antibacterial effect can reach 89.13%. The antibacterial finish with nano-zinc oxide combined with microwave features good antibacterial effect, and nano-zinc oxide can be recycled for at least twice.
出处
《上海纺织科技》
北大核心
2017年第2期19-21,共3页
Shanghai Textile Science & Technology
基金
广东省高等职业院校珠江学者岗位计划资助项目(2015)
广州市科技计划项目(201510010170)
广东轻院珠江学者人才类项目(RC2015-001)
广东省自然科学基金项目(2016A030313761)
生物无机与合成化学教育部重点实验室开放基金项目(2016)
关键词
微波技术
纳米氧化锌
羽绒
抗菌整理
microwave technique
nano-zinc oxide
down
anti-bacterial finish