期刊文献+

醋酸乙烯聚合体系热失控风险评估及失控抑制 被引量:9

Risk assessment and inhibition of thermal runaway in vinyl acetate polymerization system
原文传递
导出
摘要 为实现对醋酸乙烯(VAC)聚合反应热失控行为的风险评估及紧急抑制,采用VSP2绝热量热仪对醋酸乙烯聚合反应体系在不同危险场景条件下的热失控过程和失控抑制进行试验模拟。依据苏黎世危险性分析法(ZHA)中的失控反应严重度评估判据,评估醋酸乙烯聚合反应的热失控风险程度,提出紧急情况下抑制剂的加入时间及加入量。结果表明,醋酸乙烯聚合反应失控后绝热温升(ΔT_(ad))超过100℃,最大反应速率到达时间(TMRad)约为10 min,其热失控风险程度仅次于不可接受水平。聚合体系温度不高于73℃时,通过加入不低于参与聚合反应的醋酸乙烯质量20%的常温溶剂,可有效阻止失控反应发生。 In order to evaluate the thermal runaway risk of the VAC polymerization system and to develop an emergency inhibition methodology,an experimental study was made by using an adiabatic calorimeter VSP2. The associated runaway risk was evaluated and the proper adding time and amount of the inhibitor were determined based on the ZHA hazard analysis method. The results show that the risk is second to the most dangerous,the ΔT_(ad) is over 100 ℃,and TMRad is around 10 min,and that the runaway could be effectively suppressed by the addition of solvent( no less than 20% VAC in mass) when the system temperature is below 73 ℃.
作者 金满平 朱云峰 张婧 孙峰 徐伟 石宁 JIN Manping ZHU Yunfeng ZHANG Jing SUN Feng XU Wei SHI Ning(Institute of Chemical Process Safety, SINOPEC Research Institute of Safety Engineering, Qingdao Shandong 266071, China State Key Laboratory of Safety and Control for Chemicals, Qingdao Shandong 266071, China)
出处 《中国安全科学学报》 CAS CSCD 北大核心 2017年第1期104-109,共6页 China Safety Science Journal
关键词 醋酸乙烯(VAC) 聚合体系 热失控 风险评估 绝热温升(ΔTad) 最大反应速率到达时间(TMRad) vinyl acetate(VAC) polymerization system thermal runaway risk assessment adiabatic temperature rise(ΔTad) time to maximum rate under adiabatic condition(TMRad)
  • 相关文献

参考文献6

二级参考文献59

共引文献47

同被引文献58

引证文献9

二级引证文献20

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部