摘要
以PEG-2000为表面活性剂,与FeCl_3·6H_2O、尿素以水热法在140℃下加热18h制备β-FeOOH纳米棒。再以Na_2S_2O_8为氧化剂在溶液中进行EDOT与β-FeOOH纳米棒的包覆制备β-FeOOH@PEDOT纳米复合材料,并利用粉末X射线衍射、透射电子显微镜和红外光谱等手段对β-FeOOH@PEDOT纳米复合材料进行表征。
With PEG-2000 as the surfactant, FeCl_3·6H_2O, urea by hydrothermal method under the 140℃heating 18 hours preparation β-FeOOH nanorods. The β-FeOOH @ PEDOT nanocomposites were preparedby coating EDOT with β-FeOOH nanorods in solution with Na_2S_2O_8 as oxidant.The products have been char-acterized by X-ray diffraction, transmission electron microscopy and micro-Raman spectroscopy.
出处
《河南科技》
2017年第19期119-121,共3页
Henan Science and Technology