采用"锻造+多向轧制"工艺,研究了均质钽2.5钨合金材料在不同方向、不同部位和不同热处理工艺条件下的拉伸性能和显微组织,最终确定了均质钽2.5钨合金的加工工艺。
Homogeneous tantalum 2. 5 tungsten alloy was prepared by forging and clock rolling. Tensile properties and micro- structure of samples of different orientations, from different positions and prepared by different heat treatments were researched. Based on the tests results, the processing technology was determined.
出处
《材料开发与应用》
CAS
2017年第5期16-22,共7页
Development and Application of Materials
关键词
钽2.5钨合金
轧制
热处理
力学性能
微观组织
各向同性
Tantalum 2. 5 tungsten alloy
rolling
heat treatment
mechanical property
microstructure
isotropy