摘要
文章分别对Coolmax、Coolplus纤维织物试样和用TF-620、DM-3746进行后整理的普通涤纶织物试样的吸湿排汗性能进行了对比。结果表明水洗对后整理性织物的吸湿排汗性能影响较大,10次水洗后各项性能下降明显;永久性吸湿排汗织物(Coolmax、Coolplus纤维织物)也同样会受到水洗的影响,但影响较小,水洗10次后各项性能基本达到稳定。
This article compared the hydroscopic and sweat permeability properties of Coolmax and Coolplus fabrics,TF-620 and DM-3746 finished fabrics.Test results showed that washing significantly affected the hydroscopic and sweat permeability property of finished fabrics.After 10 times washing,the indexes were remarkably reduced.Influence of washing on permanent fabrics(Coolmax and Coolplus fabrics)was little.After 10 times washing,all the indexes became stable.
作者
吴琦
薛文良
Wu Qi;Xue Wenliang(College of Textiles,Donghua University,Shanghai 201620,China)
出处
《山东纺织科技》
2018年第2期19-22,共4页
Shandong Textile Science & Technology