摘要
ZrO_(2)-5CrMnMo composite samples were prepared by hot press sintering.When NiCoCrAlY powders were used as the bonding layer and the different mixtures of NiCoCrAlY alloy and 3YSZ (3mol% yttria stabilized zirconia) ceramic powders were used as the transition layers,the connection between zirconia ceramic and 5CrMnMo steel were strengthened.Three composite samples with different structures were fabricated by heat spraying and hot press sintering.Shear and thermal shock cycle tests were conducted to characterize connection strength and thermal shock resistance of these samples.The shear strength reached 95.69 MPa,and the heating shock cycles achieved to the maximum value of 27.7 times.Microstructures and connection interfaces were analyzed by scanning electron microscopy.The hardness and wearing resistance of 3YSZ coat and 5CrMnMo substrate were compared,and the heat insulation property of composite samples were also discussed.It is shown that these composite materials fabricated in this research are benefited to be used as squeeze casting dies.
作者
SUN Yonggen
DU Zhiming
CHEN Lili
FEI Yanhan
CHENG Yuansheng
孙永根;杜之明;CHEN Lili;FEI Yanhan;CHENG Yuansheng(National Key Laboratory for Precision Hot Processing of Metals,Harbin 150001,China;School of Materials Science and Engineering,Harbin Institute of Technology,Harbin 150001,China)
基金
Funded by the National Natural Science Foundation of China(No.51174064)。